ASM Aerospace Specification Metals Inc.
 


 

 

 

High Temperature and Nickel Alloys

 

SHEET & PLATE    ROD, BAR & FORGINGS    TUBING    TECHNICAL DATA
 

To learn more about Nickel & Cobalt Alloys click here.

 

  SIZES:

  ,010 to .160 x R/W x R/L

  .188 to 5.00 x R/W x R/L 

  TYPE   SPECIFICATIONS
  A-286   AMS-5525
  HASTELLOY C*   AMS-5530
  HASTELLOY X*   AMS-5536, B50TF24, 25, PWA-1038
  HAYNES 188*   AMS-5608, PWA-1042, B50TF74
  INCOLOY 800²   AMS-5871, ASTMB409
  INCONEL 600²   AMS-5540
  INCONEL 617²   AMS-5888, 5889, PWA-1165, B50TF181
  INCONEL 625²   AMS-5599
  INCONEL 718²   AMS-5596, 5597, B50TF14
  INCONEL 722²   AMS-5541, B50T73
  INCONEL X-750²   AMS-5542, 5598
  L-605, HAYNES 25*   AMS-5537
  N-155, MULTIMET*   AMS-5532
  NICKEL 200   ASTM-B162
  NICKEL 201   AMS-5553
  MONEL 400²   AMS-4544, ASTM B127, QQN281
  RENE 41   AMS-5545, B50TF76, B50TF109
  WASPALOY¹   AMS-5544

[return to the top of page]

 

  Full Range of

  Sizes in All Shapes

  Forgings:

  Full range of sizes

 

  TYPE   SPECIFICATIONS
  A-286   AMS-5731, 5732, 5734, 5737
  HASTELLOY C*   AMS-5750
  HASTELLOY X*   AMS-5754, B50TF31
  INCOLOY 800²   AMTMB408
  INCONEL 600²   AMS-5665
  INCONEL 625²   AMS-5666
  INCONEL 718²   AMS-5662, 5663, 5664, B50TF15, LBO170-186
  INCONEL 722²   AMS-5714
  INCONEL X-750²   AMS-5667, 5668, 5670, 5671
  L-605, HAYES 25*   AMS-5759
  N-155   AMS-5768, 5769
  NICKEL 200   ASTMB160
  MONEL 400²   ASTMB164, QQN281
  MONEL²  K500²   AMS4676, QQN286
  WASPALOY¹   AMS-5704, 5706, 5707, 5708, 5709
  INCONEL 901²   AMS-5660, 5661
  RENE 41   AMS-5712, 5713, B50TF75

[return to the top of page]


  Sizes:

  .020 to 12.00 OD

  .002 to 4.00 Wall

  TYPE   SPECIFICATIONS
  A-286   AMS-5732, 5734, 5737
  HASTELLOY X*   AMS-5587, 5588, PWA-1066
  HAYNES 188*   PWA-1088
  INCONEL 600²   AMS-5580, PWA-1060, 1070
  INCONEL 625²   AMS-5581, PWA-1069, 1072, B50TF133
  INCONEL 718²   AMS-5589, 5590, PWA-1065
  INCONEL X-750²   AMS-5582
  WASPALOY¹   AMS-5586
  L-605   B50T27

[return to the top of page]

 

Click Product to View Data

Allegheny Ludlum Altemp® A286 Iron-Base Superalloy, UNS S66286
Haynes® 188 alloy, 0% cold reduction, 3.2 mm thick sheet
Haynes® 188 alloy, 10% cold reduction, 3.2 mm thick sheet
Haynes® 188 alloy, 10% cold reduction, 3.2 mm thick sheet, 1065°C for 5 minutes
Haynes® 188 alloy, 10% cold reduction, 3.2 mm thick sheet, 1120°C for 5 minutes
Haynes® 188 alloy, 10% cold reduction, 3.2 mm thick sheet, 1175°C for 5 minutes
Haynes® 188 alloy, 20% cold reduction, 3.2 mm thick sheet
Haynes® 188 alloy, 20% cold reduction, 3.2 mm thick sheet, 1065°C for 5 minutes
Haynes® 188 alloy, 20% cold reduction, 3.2 mm thick sheet, 1120°C for 5 minutes
Haynes® 188 alloy, 20% cold reduction, 3.2 mm thick sheet, 1175°C for 5 minutes
Haynes® 188 alloy, 30% cold reduction, 3.2 mm thick sheet
Haynes® 188 alloy, 30% cold reduction, 3.2 mm thick sheet, 1065°C for 5 minutes
Haynes® 188 alloy, 30% cold reduction, 3.2 mm thick sheet, 1120°C for 5 minutes
Haynes® 188 alloy, 30% cold reduction, 3.2 mm thick sheet, 1175°C for 5 minutes
Haynes® 188 alloy, 40% cold reduction, 3.2 mm thick sheet
Haynes® 188 alloy, 40% cold reduction, 3.2 mm thick sheet, 1065°C for 5 minutes
Haynes® 188 alloy, 40% cold reduction, 3.2 mm thick sheet, 1120°C for 5 minutes
Haynes® 188 alloy, 40% cold reduction, 3.2 mm thick sheet, 1175°C for 5 minutes
Haynes® 188 alloy, cold rolled and 1175°C solution annealed sheet, tested at 1095°C (2000°F)
Haynes® 188 alloy, cold rolled and 1175°C solution annealed sheet, tested at 540°C (1000°F)
Haynes® 188 alloy, cold rolled and 1175°C solution annealed sheet, tested at 650°C (1200°F)
Haynes® 188 alloy, cold rolled and 1175°C solution annealed sheet, tested at 760°C (1400°F)
Haynes® 188 alloy, cold rolled and 1175°C solution annealed sheet, tested at 870°C (1600°F)
Haynes® 188 alloy, cold rolled and 1175°C solution annealed sheet, tested at 980°C (1800°F)
Haynes® 188 alloy, cold rolled and 1175°C solution annealed sheet, tested at RT
Haynes® 188 alloy, hot rolled and 1175°C solution annealed plate, tested at 1095°C (2000°F)
Haynes® 188 alloy, hot rolled and 1175°C solution annealed plate, tested at 1150°C (2100°F)
Haynes® 188 alloy, hot rolled and 1175°C solution annealed plate, tested at 1205°C (2200°F)
Haynes® 188 alloy, hot rolled and 1175°C solution annealed plate, tested at 540°C (1000°F)
Haynes® 188 alloy, hot rolled and 1175°C solution annealed plate, tested at 650°C (1200°F)
Haynes® 188 alloy, hot rolled and 1175°C solution annealed plate, tested at 760°C (1400°F)
Haynes® 188 alloy, hot rolled and 1175°C solution annealed plate, tested at 870°C (1600°F)
Haynes® 188 alloy, hot rolled and 1175°C solution annealed plate, tested at 980°C (1800°F)
Haynes® 188 alloy, hot rolled and 1175°C solution annealed plate, tested at RT
Haynes® 188 alloy, plate at RT after 0 hours at 650°C (1200°F)
Haynes® 188 alloy, plate at RT after 0 hours at 760°C (1400°F)
Haynes® 188 alloy, plate at RT after 0 hours at 870°C (1600°F)
Haynes® 188 alloy, plate at RT after 1000 hours at 870°C (1600°F)
Haynes® 188 alloy, plate at RT after 16000 hours at 870°C (1600°F)
Haynes® 188 alloy, plate at RT after 4000 hours at 870°C (1600°F)
Haynes® 188 alloy, plate at RT after 8000 hours at 650°C (1200°F)
Haynes® 188 alloy, plate at RT after 8000 hours at 760°C (1400°F)
Haynes® 188 alloy, plate at RT after 8000 hours at 870°C (1600°F)
Haynes® Hastelloy® X alloy, sheet, tested at 1095°C (2000°F)
Haynes® Hastelloy® X alloy, sheet, tested at 540°C (1000°F)
Haynes® Hastelloy® X alloy, sheet, tested at 650°C (1200°F)
Haynes® Hastelloy® X alloy, sheet, tested at 760°C (1400°F)
Haynes® Hastelloy® X alloy, sheet, tested at 870°C (1600°F)
Haynes® Hastelloy® X alloy, sheet, tested at 980°C (1800°F)
Haynes® Hastelloy® X alloy, sheet, tested at RT
Haynes® Multimet® alloy, 1.32 mm thick sheet, 1177°C heat treatment, rapid air cooled, tested at 1038°C
Haynes® Multimet® alloy, 1.32 mm thick sheet, 1177°C heat treatment, rapid air cooled, tested at 649°C (1200°F)
Haynes® Multimet® alloy, 1.32 mm thick sheet, 1177°C heat treatment, rapid air cooled, tested at 927°C
Haynes® Multimet® alloy, 1.32 mm thick sheet, 1177°C heat treatment, rapid air cooled, tested at RT
Haynes® Multimet® alloy, 1.6 mm thick sheet, 1177°C heat treatment, rapid air cooled, tested at 1093°C
Haynes® Multimet® alloy, 1.6 mm thick sheet, 1177°C heat treatment, rapid air cooled, tested at 1149°C (2100°F)
Haynes® Multimet® alloy, 1.6 mm thick sheet, 1177°C heat treatment, rapid air cooled, tested at 1204°C (2200°F)
Haynes® Multimet® alloy, 1.6 mm thick sheet, 1177°C heat treatment, rapid air cooled, tested at 1260°C
Haynes® Multimet® alloy, 1.6 mm thick sheet, 1177°C heat treatment, rapid air cooled, tested at 1288°C
Haynes® Multimet® alloy, 1.6 mm thick sheet, 1177°C heat treatment, rapid air cooled, tested at 427°C (800°F)
Haynes® Multimet® alloy, 1.6 mm thick sheet, 1177°C heat treatment, rapid air cooled, tested at 538°C (1000°F)
Haynes® Multimet® alloy, 1.6 mm thick sheet, 1177°C heat treatment, rapid air cooled, tested at 649°C (1200°F)
Haynes® Multimet® alloy, 1.6 mm thick sheet, 1177°C heat treatment, rapid air cooled, tested at 760°C (1400°F)
Haynes® Multimet® alloy, 1.6 mm thick sheet, 1177°C heat treatment, rapid air cooled, tested at 871°C (1600°F)
Haynes® Multimet® alloy, 1.6 mm thick sheet, 1177°C heat treatment, rapid air cooled, tested at 982°C
Haynes® Multimet® alloy, 1.6 mm thick sheet, 1177°C heat treatment, rapid air cooled, tested at RT
Haynes® Multimet® alloy, 12.7 mm (1/2 in.) thick plate, 1185°C heat treatment, water quenched, tested at -196°C
Haynes® Multimet® alloy, 12.7 mm (1/2 in.) thick plate, 1185°C heat treatment, water quenched, tested at -78°C
Haynes® Multimet® alloy, 12.7-50.8 mm hot-rolled bar, 1185°C heat treatment, water quenched, tested at RT
Haynes® Multimet® alloy, 25.4-50.8 mm forged bar, 1185°C heat treatment, water quenched, tested at RT
Haynes® Multimet® alloy, 533.4 by 82.55 mm forging, stress relieved at 649°C (1200°F), air cooled, tested at 649°C (1200°F)
Haynes® Multimet® alloy, 533.4 by 82.55 mm forging, stress relieved at 649°C (1200°F), air cooled, tested at RT
Haynes® Multimet® alloy, 6.15 mm hot-rolled bar, 10% cold reduction, tested at RT
Haynes® Multimet® alloy, 6.15 mm hot-rolled bar, 1185°C heat treatment, rapid air cooled, tested at RT
Haynes® Multimet® alloy, 6.15 mm hot-rolled bar, 15% cold reduction, tested at RT
Haynes® Multimet® alloy, 6.15 mm hot-rolled bar, 20% cold reduction, tested at RT
Haynes® Multimet® alloy, 6.15 mm hot-rolled bar, 25% cold reduction, tested at RT
Haynes® Multimet® alloy, 6.15 mm hot-rolled bar, 30% cold reduction, tested at RT
Haynes® Multimet® alloy, 6.15 mm hot-rolled bar, 35% cold reduction, tested at RT
Haynes® Multimet® alloy, 6.15 mm hot-rolled bar, 40% cold reduction, tested at RT
Haynes® Multimet® alloy, 6.15 mm hot-rolled bar, 5% cold reduction, tested at RT
Haynes® Waspaloy™ alloy, sheet, tested at 1095°C (2000°F)
Haynes® Waspaloy™ alloy, sheet, tested at 650°C (1200°F)
Haynes® Waspaloy™ alloy, sheet, tested at 760°C (1400°F)
Haynes® Waspaloy™ alloy, sheet, tested at 870°C (1600°F)
Haynes® Waspaloy™ alloy, sheet, tested at 980°C (1800°F)
Haynes® Waspaloy™ alloy, sheet, tested at RT
Nickelvac® A-286 Specialty Steel, Heat Treatment: 982°C (1800°F) + Age
Nickelvac® L-605 Nickel Superalloy, Heat Treatment: 1204°C (2200°F) Anneal
Rene 41® Nickel Superalloy, Heat Treatment: 1079°C (1975°F) + Age
Special Metals INCO® A-286 Iron-Nickel-Chromium Alloy
Special Metals INCONEL® Alloy 600
Special Metals INCONEL® Alloy 617
Special Metals INCONEL® Alloy 625
Special Metals INCONEL® Alloy 718
Special Metals INCONEL® Alloy X-750
Special Metals NIMONIC™ Alloy 901
Waspaloy® Nickel Superalloy, Heat Treatment: 1010°C (1850°F) + Age
 

 

* Trademark Haynes
¹ Trademark United Technology
² Trademark Inco Alloys
³ Trademark Carpenter

To learn more about Nickel Alloys Click Here
 